Prelithiation Activates Li(Ni0.5Mn0.3Co0.2)O2 for High Capacity and Excellent Cycling Stability.
Wu Z, Ji S, Zheng J, Hu Z, Xiao S, Wei Y, Zhuo Z, Lin Y, Yang W, Xu K, Amine K, Pan F.
Wu Z, et al.
Nano Lett. 2015 Aug 12;15(8):5590-6. doi: 10.1021/acs.nanolett.5b02246. Epub 2015 Jul 21.
Nano Lett. 2015.
PMID: 26182195
Previously, we reported a composite Li(Ni0.5Mn0.3Co0.2)O2 (NMC532) depolarized by the embedded carbon nanotube (CNT) and achieved capacity close to the theoretical limit [Wu, Z., et al. Nano. Lett. 2014, 14, 4700-4706]; unfortunately, this high capacity failed to be …
Previously, we reported a composite Li(Ni0.5Mn0.3Co0.2)O2 (NMC532) depolarized by the embedded carbon nanotube (CNT) and achieved capacity c …